WEBVTT

00:35.137 --> 00:38.840
(music)

00:38.840 --> 00:40.600
Thenumerous medical benefits

00:40.600 --> 00:42.671
of printing three-dimensional opaque

00:42.671 --> 00:47.000
or colored medical molds andmodels can be accomplished

00:47.000 --> 00:49.630
through Binder Jetting technology.

00:49.630 --> 00:52.509
At Walter Reed NationalMilitary Medical Center,

00:52.509 --> 00:55.925
technicians design objectswhich include veins,

00:55.925 --> 00:58.830
arteries, and other pathology

00:58.830 --> 01:03.115
where color can emphasize adistinct anatomical feature.

01:03.115 --> 01:05.180
(music)

01:05.180 --> 01:08.135
Binder Jetting printers use two materials;

01:08.135 --> 01:12.023
a powder, typically gypsum, and a binder.

01:14.770 --> 01:16.830
Once the technician loads the model

01:16.830 --> 01:19.115
from an external software program,

01:19.115 --> 01:21.440
the printing process begins

01:21.440 --> 01:23.653
on a platform of layered powder.

01:24.920 --> 01:27.140
Multiple print heads move horizontally

01:27.140 --> 01:30.297
along the X and Y axisof the build surface,

01:30.297 --> 01:34.403
applying a bonding agentand color to the powder.

01:36.170 --> 01:39.740
As the material hardens,the platform lowers

01:39.740 --> 01:43.840
and a new layer of gypsumis drawn across the bed.

01:43.840 --> 01:47.310
Throughout this process theobject is self-supported

01:47.310 --> 01:52.310
within the powder bed, andonce the part is completed,

01:52.467 --> 01:56.490
the remaining unboundmaterial can be eliminated

01:56.490 --> 01:59.617
with a vacuum and then recycled.

01:59.617 --> 02:02.620
(music)

02:02.620 --> 02:05.630
Upon removing the fragilemodel from the bed,

02:05.630 --> 02:08.910
the operator clears awaymost of the surface powder

02:09.920 --> 02:12.153
by using a brush or a vacuum.

02:13.740 --> 02:18.660
Then, any remaining residualmaterial is blown off

02:18.660 --> 02:21.713
with compressed air insidean enclosed chamber.

02:22.940 --> 02:25.040
Once this process is completed,

02:25.040 --> 02:26.620
the brittle surface is hardened

02:26.620 --> 02:29.900
by applying a layer of cyanoacrylate,

02:29.900 --> 02:34.063
a strong, fast acting adhesive,over the entire object.

02:35.102 --> 02:36.890
Due to the sensitive nature

02:36.890 --> 02:38.790
of the binding materials utilized

02:38.790 --> 02:43.090
in Binder Jetting technology,these systems are best suited

02:43.090 --> 02:46.100
to service patients,by the fabrication of molds

02:46.100 --> 02:49.678
for facial prosthesis, aswell as supporting providers

02:49.678 --> 02:53.440
through the building of coloredanatomical training models

02:53.440 --> 02:55.451
and medical simulators.

02:55.451 --> 02:58.451
(music)